Cobalt based high temperature alloy that can be deformed into profiles or parts blanks by overheating or (and) cold working. Adding about 20% nickel to the cobalt matrix to form a stable γ Austenite matrix; Add about 20% Cr to improve oxidation resistance and corrosion resistance; Add about 15% of W as the main solid solution strengthening element for solid solution strengthening.
Metals -> Special purpose metals -> Superalloys